Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 121 MPa | 17500 psi | 132/10s; ISO 2039 |
Borealis GD310U Polypropylene Compound, Glass Fiber Reinforced GD310U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |