Polymer Property : Ball Indentation Hardness = 220 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 220 MPa
31900 psi
dry; ISO 2039-1
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50
Product Description: Grilamid 1SBVX-50H LDS black is a 50% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno..
Ball Indentation Hardness 220 MPa
31900 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-35 PA666-GF35
Information provided by EMS Grivory
Ball Indentation Hardness 220 MPa
31900 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-35/4 H black 9836 PA666-GF35
Product description: Grilon TSG-35/4 H is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Ball Indentation Hardness 220 MPa
31900 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-35/4 PA666-GF35
Product description: Grilon TSG-35/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers. Grilon TSG-35/4 has the following important properties: Good flo..
Ball Indentation Hardness 220 MPa
31900 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35
Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Ball Indentation Hardness 220 MPa
31900 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4101 black 9225 PA*-GF40
Product description: Grivory XE 4101 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia..
Ball Indentation Hardness 220 MPa
31900 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4108 black 9992 PA612-GF50
Product description: Grilamid XE 4108 black 9992 is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorpti..
Ball Indentation Hardness 220 MPa
31900 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4108 nat PA612-GF50
Product description: Grilamid XE 4108 natural is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorptiong..
Ball Indentation Hardness 220 MPa
31900 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BGZ-40 PA6-GF40
Product description: Grilon BGZ-40 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 40% glass fibers. Grilon BGZ-40 has the following important properties:..
Ball Indentation Hardness 220 MPa
31900 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 5051 (BGZ-40 FC) PA6-GF40
Product description: Grilon XE 5051 is a impact modified, heat stabilized PA 6 injection molding grade with 40% glass fiber reinforcement. Grilon XE 5051 has the following important properties: High..
Ball Indentation Hardness 220 MPa

@Load 36.5 kg
31900 psi

@Load 80.5 lb
ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF10 MX6 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T..
Ball Indentation Hardness 220 MPa

@Load 36.5 kg
31900 psi

@Load 80.5 lb
ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV2 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grade, flammability class V2, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning...
Ball Indentation Hardness 220 MPa
31900 psi
ISO 2039-1
BASF Ultradur® B 4406 G6 30% Glass Filled PBT
Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh..
Ball Indentation Hardness 220 MPa

@Load 98.0 kg,
Time 30.0 sec
31900 psi

@Load 216 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultradur® B 4300 G10 50% Glass Filled PBT
Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou..