Ball Indentation Hardness 158 MPa
22900 psi
ISO 2039-1
Nilit FRIANYL B63 SG-GV 2010 Nylon 6 for injection molding, 20% mineral filled and 10% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 158 MPa
22900 psi
ISO 2039-1
Nilit FRIANYL B63 W-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 158 MPa
22900 psi
ISO 2039-1
Nilit FRIANYL B63 W-SG-GV 2010 Nylon 6 for injection molding, 20% mineral filled, 10% glass fiber reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics