Nilit FRIANYL B63 W-SG-GV 2010 Nylon 6 for injection molding, 20% mineral filled, 10% glass fiber reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Nilit (formerly Frisetta Polymer)
Trade Name FRIANYL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nilit FRIANYL B63 W-SG-GV 2010 Nylon 6 for injection molding, 20% mineral filled, 10% glass fiber reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Water Absorption 1.0 - 2.0 %
1.0 - 2.0 %
ISO 62
Water Absorption at Saturation 6.0 - 7.0 %
6.0 - 7.0 %
ISO 62
Viscosity Measurement 145
145
Viscosity index; ISO 307
Linear Mold Shrinkage 0.0090 - 0.019 cm/cm
0.0090 - 0.019 in/in
FRISETTA Test Method
Mechanical Properties Metric English Comments
Ball Indentation Hardness 158 MPa
22900 psi
ISO 2039-1
Tensile Strength at Break 110 MPa
16000 psi
ISO 527
Elongation at Break 3.5 %
3.5 %
ISO 527
Tensile Modulus 6.00 GPa
870 ksi
ISO 527
Flexural Strength 135 MPa
19600 psi
ISO 178
Flexural Modulus 5.00 GPa
725 ksi
ISO 178
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
DIN 53453
4.50 J/cm²
21.4 ft-lb/in²
ISO 179/1eU
2.70 J/cm²

@Temperature -40.0 °C
12.8 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
0.600 J/cm²
2.86 ft-lb/in²
DIN 53453
0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
0.700 J/cm²

@Temperature -40.0 °C
3.33 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ISO 3146 DSC
Maximum Service Temperature, Air 105 °C
221 °F
Continuous; FRISETTA Test Method
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 93
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 400 V
400 V
CTI 100; IEC 112