Ball Indentation Hardness 164 MPa
23800 psi
H358/30; ISO 2039-1
Chi Mei Kibisan® PN-127 SAN
Heat Resistant
Ball Indentation Hardness 164 MPa
23800 psi
H358/30; ISO 2039-1
Chi Mei Kibisan® PN-127H SAN
Chemical Resistant
Ball Indentation Hardness 164 MPa

@Load 36.5 kg,
Time 30.0 sec
23800 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
BASF Ultraform® N2200 G43 POM
Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF
Ball Indentation Hardness 164 MPa
23800 psi
ISO 2039-1
BASF Ultradur S 4090 G6 30% Glass Filled PBT
Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati..
Ball Indentation Hardness 164 MPa
23800 psi
GB3398
Beijing Evergrow Resources MC Nylon
Information provided by Beijing Evergrow Resources.