Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 28.0 MPa | 4060 psi | 132 N/10S; ISO 2039 |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Ball Indentation Hardness | 28.0 MPa | 4060 psi | H385/30; ISO 2039 |
Borealis Daplen™ SB4411/2 Polypropylene Compound Elastomer and Mineral Modified Daplen SB4411/2 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. The product is available in black, but other colors can be provided on request.Daplen .. |