Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 4930 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 34.0 MPa
4930 psi
ISO 2039-1
Quadrant EPP TIVAR® 1000 antistatic PE-UHMW + carbon black (ISO Data)
By incorporating an effective carbon black grade, TIVAR 1000 antistatic offers the electrostatic dissipative properties often required for PE-UHMW components operating at high line speeds and convey..
Ball Indentation Hardness 34.0 MPa
4930 psi
ISO 2039-1
Quadrant EPP TIVAR® 1000 ASTL PE-UHMW + specific additives (ISO Data)
TIVAR 1000 ASTL, based on a PE-UHMW grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion..
Ball Indentation Hardness 34.0 MPa
4930 psi
ISO 2039-1
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data)
TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl..
Ball Indentation Hardness 34.0 MPa
4930 psi
ISO 2039-1
Quadrant EPP TIVAR® ECO PE-UHMW reprocessed (ISO Data)
This grade, partially composed of reprocessed PE-UHMW material, has an overall lower property level than the virgin TIVAR 1000 and a lower cost. Compared with virgin PE 500, however, it has a much b..
Ball Indentation Hardness 34.0 MPa
4930 psi
ISO 2039-1
Azoty Tarnow™ TARFLEN SG-2 PTFE
Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 34.0 MPa
4930 psi
ISO 2039-1
Azoty Tarnow™ TARFLEN SM-1 PTFE
Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 34.0 MPa
4930 psi
ISO 2039-1
Azoty Tarnow™ TARFLEN SM-2 PTFE
Non Free Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 34.0 MPa
4930 psi
ISO 2039-1
Azoty Tarnow™ TARFLEN ST PTFE
Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 34.0 - 36.0 MPa
4930 - 5220 psi
ISO 2039-1
Adamas Hardor® 991 PE-UHMW
Information provided by Adamas, HPM
Ball Indentation Hardness 34.0 - 40.0 MPa
4930 - 5800 psi
DIN 53 456
Isoflon ETFE
Fluoropolymer material specifications.Information provided by Isoflon.
Copyright © lookpolymers.com All Rights Reserved