Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 55.0 MPa | 7980 psi | ISO2039.1 DIN.53456 |
Omnia Plastica PE 300 - Polyethylene 300 Molecular weight 300,000 polyethylene similar to the type 500 with higher rigidity and lower resistance to continuous shocks. The applications are similar to those of PE 500, being more commonly spe.. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | ISO 2039-1 |
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | ISO 2039-1 |
Quadrant EPP Fluorosint® MT-01 PTFE + additives, enhanced grade, compression moulded (ISO Data) Fluorosint MT-01 is an extreme service grade developed specifically for applications where the benefits of PTFE-based materials also require strength, stiffness and stability. Fluorosint MT-01 deliv.. |
|||
Ball Indentation Hardness | 55.0 - 195 MPa | 7980 - 28300 psi | Average value: 126 MPa Grade Count:4 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | ISO 2039 |
GEHR Plastics PE-ELS® Polyethylene HDPE A variant of PE-HD with improved electrical conductivity.Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties a.. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | DIN 53456 |
Global PP-2500-H Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-crates, pallets, paint drum, storage & transport container, seatsInformation provided by Global Po.. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | DIN 53456 |
Global PP-2512-H Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-special for wire & cable, telecom insulationInformation provided by Global Polymers Corporation. |
|||
Ball Indentation Hardness | 55.0 - 65.0 MPa | 7980 - 9430 psi | DIN 53 456 |
Isoflon ECTFE Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | ISO 2039-1 |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® AZ 3 PA66 Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures.. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® AZ 3/2 PA66 Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE.. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BS PA6 Product description: Grilon BS is an unreinforced, heat stabilized standard PA6 injection molding grade with normal melt viscosity. Grilon BS has the following important properties: Good flow behavi.. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® EB 50 H PA6 Product description: Grilon EB 50 H is a high viscosity, unreinforced, heat stabilized PA6 extrusion blow mounding grade. Grilon EB 50 H has the following important properties: High melt strengthImp.. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® L 25 Z PA12-I Product Description: Grilamid L 25 Z is a UV- and heat stabilized high viscosity polyamide 12 grade with improved toughness. A special feature of Grilamid L25 Z is its high energy absorption capacit.. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril.. |
|||
Ball Indentation Hardness | 55.0 MPa | 7980 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BR 40 W PA6 Product description: Grilon BR 40 W is a medium viscosity, plasticized PA6 extrusion grade. Grilon BR 40 W has the following important properties: High flexibilityHigh stiffness Grilon BR 40 W is us.. |