Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 60.0 MPa | 8700 psi | ISO 2039-1 |
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data) Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig.. |
|||
Ball Indentation Hardness | 60.0 - 120 MPa | 8700 - 17400 psi | Average value: 82.9 MPa Grade Count:24 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Ball Indentation Hardness | 60.0 MPa | 8700 psi | Fm=358N; Ø 50x4mm; ISO 2039-1 |
SYNTHOS Krasten® 662E High Impact Polystyrene High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of demanding visual appearance plates, technical parts, sheets and molded pa.. |
|||
Ball Indentation Hardness | 60.0 MPa | 8700 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® AS LF 20 PA66-Z20 Product description: Grilon AS LF 20 is a heat stabilized, normal viscosity PA 66 injection molding grade with 20% lubricant (PTFE + silicon oil). Grilon AS LF 20 has the following important propert.. |
|||
Ball Indentation Hardness | 60.0 MPa | 8700 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BS EC PA6 Product description: Grilon BS 23 is an unreinforced, low viscosity and fine crystalline PA 6 injection molding grade. Grilon BS 23 has the following important properties: Good flow behaviorEasy pro.. |
|||
Ball Indentation Hardness | 60.0 MPa | 8700 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BS/2 PA6 Product description: Grilon BS/2 is an unreinforced, nucleated standard PA6 injection molding grade with normal melt viscosity. Grilon BS/2 has the following important properties: Good flow behavior.. |
|||
Ball Indentation Hardness | 60.0 MPa | 8700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4128 black 9221 PA610 Product description: Grilamid XE 4128 black 9221 is a modified high viscosity Polyamide 610 for extrusion as well as injection molding. A characteristic of tubes made out of this material is the hig.. |
|||
Ball Indentation Hardness | 60.0 MPa | 8700 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BR 40 PA6 Product description: Grilon BR 40 is a medium viscosity, unreinforced, heat stabilized PA6 grade for injection mounding and extrusion applications. Grilon BR 40 has the following important propertie.. |
|||
Ball Indentation Hardness | 60.0 - 64.0 MPa | 8700 - 9280 psi | ISO 2032-N132 |
Adamas Adalon® 992 Modified PTFE Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 60.0 - 140 MPa | 8700 - 20300 psi | Average value: 100 MPa Grade Count:4 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Ball Indentation Hardness | 60.0 MPa | 8700 psi | 358 N/30s; ISO 2039 |
Borealis ME268Al Polypropylene Compound, Mineral Filled ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par.. |
|||
Ball Indentation Hardness | 60.0 - 62.0 MPa | 8700 - 8990 psi | ISO 2032 |
Adamas Adalon® 510 PTFE, 5% MoS2 Information provided by Adamas, HPM |