Mechanical Properties Metric English Comments
Ball Indentation Hardness 63.0 MPa
9140 psi
DIN 53456
Global PP-2300-LC Polypropylene Block Copolymer
Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polyme..
Ball Indentation Hardness 63.0 MPa
9140 psi
132 N/10s; ISO 2039
Borealis Daplen™ EF341AE Polypropylene TPO Compound
Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..