Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 44.0 - 48.0 MPa | 6380 - 6960 psi | ISO 2032-N132 |
Adamas Adalon® 215 PTFE, 17% Glass Filled, Blue Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 42.0 - 48.0 MPa | 6090 - 6960 psi | ISO 2032-N132 |
Adamas Adalon® 436 PTFE, 15% Ekonol® Information provided by Adamas, HPM |