Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 90.0 - 230 MPa | 13100 - 33400 psi | Average value: 192 MPa Grade Count:8 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Ball Indentation Hardness | 90.0 - 320 MPa | 13100 - 46400 psi | Average value: 194 MPa Grade Count:5 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Ball Indentation Hardness | 90.0 - 225 MPa | 13100 - 32600 psi | Average value: 173 MPa Grade Count:16 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039 |
GEHR Plastics PA 12 TR Transparent Nylon 12 Used for optical components that benefit from the transparency and the high dynamic strengthProperties:TransparencyExtremely high dynamic strengthHigh chemical resistanceHigh stress-cracking resista.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039-1 |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | Conditioned; ISO 2039-1 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Ball Indentation Hardness | 90.0 MPa @Load 36.5 kg, Time 30.0 sec |
13100 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S 757 G UV White 37019 ASA Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039-1 |
Styrolution Novodur® M210TF ABS Novodur M210TF is medium impact, high gloss injection molding grade designed for toy application. M210TF is in compliance with food contact regulationsInformation provided by Styrolution |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039-1 |
Styrolution PS 454N HIPS Styrolution PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Good balance of toughness, high flow, and heat resistanceHigh gloss.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039-1 |
Styrolution PS 641F HIPS Styrolution PS 641F is high impact polystyrene with high heat resistance.High impactHigh heat resistanceInformation provided by Styrolution |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | H 385/30; ISO 2039 |
Borealis Xmod™ HF006SA High Stiffness Polypropylene for Injection Molding Applications Xmod HF006SA is a high melt flow PP homopolymer with increased crystallinity, intended for injection molding. Xmod HF006SA is specifically developed for applications demanding a high surface appear.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® B 70 GFE 30 H PA6-GF30 Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important p.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-25 HM PA6-GF25 Product description: Grilon BG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 25% glass fibers. Grilon BG-25 HM has the following important prop.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-25 S PA6-GF25 Product description: Grilon BG-25 S is a heat stabilized PA6 injection molding grade with 25 % glass fibers. Grilon BG-25 S has the following important properties: Excellent surface finishEasy flowi.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30 Product description: Grilon BGM-30 X is a heat stabilized PA 6 injection molding grade with a 30 % reinforcement combination (mineral and glass fiber). Grilon BGM-30 X has the following important pr.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® R 50 H NZ PA6 Product description: Grilon R 50 H NZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon R 50 H NZ has the following important properties: V.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSM-30 PA666-MD30 Product description: Grilon TSM-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral. Grilon TSM-30 has the following important properties: Excellent surface.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSZ 3 PA666 Product description: Grilon TSZ 3 is a heat stabilized, normal viscosity, high impact modified PA66 + PA6 injection molding grade. Grilon TSZ 3 has the following important properties: Excellent toug.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 3997 nat PAMACM12 Product description: Grilamid XE 3997 natural is a transparent thermoplastic polyamide based on aliphatic and cycloaliphatic blocks. Grilamid XE 3997 natural is particularly suitable for blow molded.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | H358/30; ISO 2039-1 |
Chi Mei Polyrex® PH-60 Polystyrene - High Impact Medium impact |
|||
Ball Indentation Hardness | 90.0 MPa @Time 30.0 sec |
13100 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PA 11 Nylon 11 Water armatures, bearing under water, seals, housings, fans, insulated parts, parts for textile machines and household units. Toother wheels, sliding components and guides. Very low water absorpti.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BGZ-30 PA6-GF30 Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TR 90 LS PAMACM12 Product description: Grilamid TR 90 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LS natural contains a processing a.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | H358/30; ISO 2039-1 |
Chi Mei Polylac® PA-758 ABS - Transparent Transparent |
|||
Ball Indentation Hardness | 90.0 MPa @Load 36.5 kg |
13100 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 MCS HI Polyamide 6 - Impact Modified Very high impact resistance, cold impact grade (to -40°C). Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has t.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 300 CI4 POM Impact modified injection molding grade based on Tarnoform 300 reinforced with 20% MBS rubber yielding good cold impact strength and good strength of weld lines combined with good weatherability.Inf.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | ISO 2039-1 |
Covestro Makroblend® UT4045 G PC/PBT Blend, 20% Glass Filled Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Excellent chemic.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TR 55 LZ PA12/MACMI Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LZ offers a variety of interesting properties such as: c.. |
|||
Ball Indentation Hardness | 90.0 MPa | 13100 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTROLEN PP TV Polypropylene + talc This material is a low density, easily machined plastic that has good damping properties and is reinforced with talc for high rigidity. Applications include components for the electrical industry, h.. |