Hippe PA 11 Nylon 11

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Unreinforced
Manufacturer Erhard Hippe KG
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PA 11 Nylon 11.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Water armatures, bearing under water, seals, housings, fans, insulated parts, parts for textile machines and household units. Toother wheels, sliding components and guides. Very low water absorption.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
DIN 53 479
Moisture Absorption at Equilibrium 0.90 %
0.90 %
Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation 1.9 %
1.9 %
DIN 53 495
Mechanical Properties Metric English Comments
Ball Indentation Hardness 90.0 MPa

@Time 30.0 sec
13100 psi

@Time 0.00833 hour
DIN 53 456
Tensile Strength 42.0 MPa
6090 psi
cond.; DIN 53 455
47.0 MPa
6820 psi
dry; DIN 53 455
Elongation at Break 230 %
230 %
dry; DIN 53 455
280 %
280 %
cond.; DIN 53 455
Tensile Modulus 1.80 GPa
261 ksi
DIN 53 457
Charpy Impact, Notched NB
NB
DIN 53 453
Coefficient of Friction, Dynamic 0.32 - 0.38
0.32 - 0.38
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Abrasion 0.80
0.80
µm/km; Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C
55.6 µin/in-°F
Specific Heat Capacity 2.10 J/g-°C
0.502 BTU/lb-°F
Thermal Conductivity 0.230 W/m-K
1.60 BTU-in/hr-ft²-°F
Melting Point 183 °C
361 °F
DIN 53 736
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous use
150 °C
302 °F
Short Periods
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO-R 75 Method A
Glass Transition Temp, Tg 43.0 °C
109 °F
dynamic; DIN 53 736
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
DIN 53 482, VDE 0303, Part 3
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
DIN 53 482
Dielectric Constant 3.6

@Frequency 1.00e+6 Hz
3.6

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 40.0 kV/mm
1020 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.040

@Frequency 1.00e+6 Hz
0.040

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Color natural
Creep Resistance Grade CTI 600
DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, suds resistant