Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0345 - 0.0758 MPa

@Strain 25.0 %
5.00 - 11.0 psi

@Strain 25.0 %
Range, 0.2"/min. strain rate
Rogers Corporation Poron® 4701-41-15 Urethane Foam, Soft, Enhanced Sealability
Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements.  Standard available thickness range from 0.031"..