Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0827 MPa @Strain 4.00 % |
12.0 psi @Strain 4.00 % |
Load applied normal to fiber plane |
Zircar Ceramics ALC Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Compressive Yield Strength | 0.0830 MPa @Strain 10.0 % |
12.0 psi @Strain 10.0 % |
BS ISO 7214 1998 |
Zotefoams Evazote® EV70CN Conductive Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Compressive Yield Strength | 0.0830 MPa @Strain 40.0 % |
12.0 psi @Strain 40.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® LD24FR Low Density Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |