Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1420 MPa @Temperature 23.0 °C |
206000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 1420 MPa @Temperature 24.0 °C |
206000 psi @Temperature 75.2 °F |
|
Hexcel® HexPly® F263 Epoxy Resin, T3T095 Carbon Tape Hexcel designation: T_095-12"-F263; Various fibersInformation provided by HexCel |