Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber

Category Polymer , Thermoset , Epoxy
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2680 MPa

@Temperature 23.0 °C
389000 psi

@Temperature 73.4 °F
Tensile Modulus 160 GPa

@Temperature 23.0 °C
23200 ksi

@Temperature 73.4 °F
Flexural Yield Strength 87.6 MPa

@Temperature 23.0 °C
12700 psi

@Temperature 73.4 °F
Compressive Yield Strength 207 MPa

@Temperature 23.0 °C
30000 psi

@Temperature 73.4 °F
216 MPa

@Temperature 177 °C
31300 psi

@Temperature 351 °F
Open Hole Compression; Wet
224 MPa

@Temperature 163 °C
32500 psi

@Temperature 325 °F
Open Hole Compression; Wet
236 MPa

@Temperature 149 °C
34200 psi

@Temperature 300 °F
Open Hole Compression; Wet
285 MPa

@Temperature 23.0 °C
41300 psi

@Temperature 73.4 °F
1000 MPa

@Temperature 163 °C
145000 psi

@Temperature 325 °F
1030 MPa

@Temperature 177 °C
149000 psi

@Temperature 351 °F
1410 MPa

@Temperature 149 °C
205000 psi

@Temperature 300 °F
0°, Wet
1420 MPa

@Temperature 23.0 °C
206000 psi

@Temperature 73.4 °F
Shear Modulus 2.76 GPa

@Temperature 163 °C
400 ksi

@Temperature 325 °F
In-Plane; Wet
2.90 GPa

@Temperature 149 °C
421 ksi

@Temperature 300 °F
In-Plane; Wet
4.27 GPa

@Temperature 23.0 °C
619 ksi

@Temperature 73.4 °F
Shear Strength 46.2 MPa

@Temperature 163 °C
6700 psi

@Temperature 325 °F
Short Beam, Wet
48.3 MPa

@Temperature 149 °C
7010 psi

@Temperature 300 °F
Short Beam, Wet
49.6 MPa

@Temperature 177 °C
7190 psi

@Temperature 351 °F
Short Beam
49.6 MPa

@Temperature 177 °C
7190 psi

@Temperature 351 °F
Short Beam, Wet
58.6 MPa

@Temperature 163 °C
8500 psi

@Temperature 325 °F
Short Beam
63.4 MPa

@Temperature 149 °C
9200 psi

@Temperature 300 °F
Short Beam
100 MPa

@Temperature 23.0 °C
14500 psi

@Temperature 73.4 °F