Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 17.0 MPa @Strain 1.00 % |
2470 psi @Strain 1.00 % |
dry; ISO 604 |
Murtfeldt Murinyl® Polyvinylidinefluoride As a fluorinated plastic, Murinyl® is exceptionally resistant to chemicals, hydrolysis, and sterilization. Its properties change very little at high service temperatures and after long-term exposur.. |