Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 165 MPa @Temperature 71.0 °C |
23900 psi @Temperature 160 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, K120 Kevlar Fabric Fiber: Kev. 49 195Information provided by HexCel |