Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 30000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 207 MPa

@Temperature 23.0 °C
30000 psi

@Temperature 73.4 °F
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber
Information provided by HexCel
Compressive Yield Strength 207 MPa

@Strain 23.0 %
30000 psi

@Strain 23.0 %
at max stress; ASTM D695
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Compressive Yield Strength 207 MPa

@Strain 27.0 %
30000 psi

@Strain 27.0 %
at max stress; ASTM D695
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Compressive Yield Strength 207 MPa

@Strain 10.0 %,
Temperature 23.0 °C
30000 psi

@Strain 10.0 %,
Temperature 73.4 °F
ASTM D695 Modified
Saint-Gobain Meldin® 2021 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..