Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 32.0 MPa @Strain 2.00 % |
4640 psi @Strain 2.00 % |
dry; ISO 604 |
Murtfeldt Murinyl® Polyvinylidinefluoride As a fluorinated plastic, Murinyl® is exceptionally resistant to chemicals, hydrolysis, and sterilization. Its properties change very little at high service temperatures and after long-term exposur.. |
|||
Compressive Yield Strength | 32.0 MPa @Strain 1.00 % |
4640 psi @Strain 1.00 % |
dry; ISO 604 |
Murtfeldt Murylon® A Nylon 66 This material combines the excellent properties of the Murylon® range with additional high tensile and compressive strength, increased wear resistance, and a lower level of moisture absorption than.. |