Polymer Property : Compressive Yield Strength = 50000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 345 MPa

@Temperature 25.0 °C
50000 psi

@Temperature 77.0 °F
After 1500 in-inlb/in impact
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber
Information provided by HexCel
Compressive Yield Strength 345 MPa

@Temperature 25.0 °C
50000 psi

@Temperature 77.0 °F
After 500 in-in-lb/in impact, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Information provided by HexCel
Compressive Yield Strength 345 MPa

@Temperature 163 °C
50000 psi

@Temperature 325 °F
0°, Wet (Immersed in water at 71°C for 7 days)
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric
Information provided by HexCel
Compressive Yield Strength 345 MPa

@Temperature 149 °C
50000 psi

@Temperature 300 °F
0°, Wet
Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric
Information provided by HexCel
Compressive Yield Strength 345 MPa

@Temperature 177 °C
50000 psi

@Temperature 351 °F
Hexcel® HexPly® F263 Epoxy Resin, 120 Glass Fabric
Hexcel designation: 120-38"-F263; Fiber: 450-1/2Information provided by HexCel