Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 350 MPa @Temperature 90.0 °C |
50800 psi @Temperature 194 °F |
0°, Conditioning: 23°C; ASTM D965 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 6K High Strength Carbon Fiber Designation: C370S5, Satin weave, 5HInformation provided by HexCel |