Mechanical Properties Metric English Comments
Compressive Yield Strength 45.0 MPa

@Strain 2.00 %
6530 psi

@Strain 2.00 %
dry; ISO 604
Murtfeldt Murylon® HT Nylon 46
The use of this highly temperature resistant polyamide enables reliable operation up to a constant service temperature of 155°C . The material retains its rigidity and creep strength over the entir..