Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Sorona® FG3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data** Sorona® FG3015G NC010 is a 15% glass fiber reinforced polytrimethylene terephthalate resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) formulated to be food c.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 GV 5 Nylon 6.6 for injection molding, 5% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 84 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets, High Mechanical Strength
& Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, moldin.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® C 216 V15 PA6, 15% glass filled, Eh 0 Description: TECHNYL C 216 V15 is a polyamide 6 with 15% of glass fiber.Colors: it is marketed in the black color and natural.Available in: Asia Pacific and EuropeMain Properties: Dimensional stabil.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ KSR4525 Polypropylene Reactor Elastomer Modified Daplen KSR4525 is a reactor elastomer modified polypropylene intended for injection molding. Daplean KSR4525 is a material with excellent impact/stiffness ratio. The grade is available in natural .. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis HB205TF Polypropylene HB205TF is a low melt flow rate polypropylene homopolymer intended for extrusion, calendering and thermoforming. Its very good organoleptic properties allows this grade to be used with any master b.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179 |
Total PPC 9642 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9642 is nucleated heterophasic copolymer. PPC 9642 is characterized by improved stiffness, creep resistance, high impact resistance, excellent antistatic properties and has been f.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PA-A4 Flame-Retardant & Mineral Reinforced PA6 Applications: Top Grad CBInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT) 15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on pol.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | dry; ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-29 MS Polyamide 6 - Natural Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.For .. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | dry; ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-29 Polyamide 6 - Natural Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.Tarn.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAFORM C 520.0 POM Copolymer unreinforced POMInformation provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addilene J 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Sorona® FG3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data** 15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Developed for Food Contact Applications Sorona FG3015G NC010 is a 15% glass fiber reinforced polytrimethylene terephthalate resi.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/IeA |
Addiplast Addinyl C2 V15 Nylon 66/6, 15% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179 |
BASF Ultraform S 1320 0021 UNC POM Ultraform S1320 0021 UNC is an easy flowing, rapidly freezing injection molding POM grade with enhanced stiffness and heat distortion resistance. It is highly stabilized to resist aggressive fuels,.. |
|||
Charpy Impact, Notched | 0.550 J/cm² - NB @Temperature -30.0 - -30.0 °C |
2.62 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Average value: 1.35 J/cm² Grade Count:48 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® M140-44/M140S Acetal Co-polymer (POM), Standard, High flow DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |