Material Notes:
Description: TECHNYL C 216 V15 is a polyamide 6 with 15% of glass fiber.Colors: it is marketed in the black color and natural.Available in: Asia Pacific and EuropeMain Properties: Dimensional stability, Impact resistance and Stiffness Applications: TECHNYL C 218 V15 was developed for applications on parts where good mechanical properties as impact resistance, superficial aspect and dimensional stability are required.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183/A
Water Absorption 1.15 %

@Temperature 23.0 °C,
Time 86400 sec
1.15 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
ISO R 527
Elongation at Break 4.0 %
4.0 %
ISO R 527
Tensile Modulus 6.10 GPa
885 ksi
ISO R 527
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 4.20 J/cm²
20.0 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²
2.62 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
ISO 75-2
Flammability, UL94 HB
HB
Oxygen Index 23 %
23 %
ISO 4589
Glow Wire Test 650 °C

@Thickness 1.60 mm
1200 °F

@Thickness 0.0630 in
CEI 695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
CEI 93
Dielectric Constant 3.8
3.8
CEI 250
Dissipation Factor 0.020
0.020
CEI 250
Comparative Tracking Index 550 V
550 V
CEI 112
Processing Properties Metric English Comments
Feed Temperature 225 - 230 °C
437 - 446 °F
Nozzle Temperature 230 - 240 °C
446 - 464 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Descriptive Properties Value Comments
Compression Zone 230-240°C
Mixing Zone 230-240°C