Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 KV30 Nylon 6 for injection molding, 30% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Ertacetal® C POM-C, extruded (ISO Data) Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant compos.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eA |
Pasargad Polymer Peyvand Pasalen 3P-H3230B Polypropylene, 30% Mineral Filled Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
Polimeri Europa EDISTIR RC3 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-18 Special high impact, high gloss polystyrene grade. Suitable for injection molding in the appliances sector.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 19-7277 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
LATI Latamid 66 H2 G/25-V0KB1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
LATI Latiohm 62-08 PD02 G/30 PPA, 30% Glass Fiber Reinforced Dissipative product based on Polyamide 6 (PA6). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179 |
Solvay TECHNYL® C 218L V30 PA6, 30% glass fiber, Eh 0 Description: TECHNYL C 218 L V30 is a polyamide 6 reinforced with 30% glass fiber and UV stabilized.Colors: it is marketed in the natural and black color.Available in: Latin America Main Properties:.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179-1 |
Unitika A175G15 PA66, 15% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature -20.0 °C |
3.81 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Total PPC 3640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 3640 is a nucleated heterophasic copolymer. PPC 3640 is characterized by improved stiffness, creep resistance and high impact resistance.ApplicationPPC 3640 has been devel.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® AS V0 PA66 Product description: Grilon AS V0 is an unreinforced, normal viscosity, self-extinguishing PA66 injection molding grade. Grilon AS V0 has the following important properties: Halogen and phosphorous-.. |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® TSC-20/4 EC black 9832 PA666-CF20 Information provided by EMS Grivory |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature 30.0 °C |
3.81 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-35/4 H black 9836 PA666-GF35 Product description: Grilon TSG-35/4 H is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 4028 nat PA12/MACMI Product description: Grilamid XE 4028 natural is a transparent thermoplastic polyamides based on aliphatic, cycloaliphatic and aromatic blocks. Grilamid XE 4028 natural offers a variety of interesti.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® SK645FR BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR BK851 is a flame retardant 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL.. |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 525GR NC000 Acetal (POM)
(Unverified Data**) 25% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 525GR NC000 is a 25% glass reinforced acetal homopolymer for injection molding. It has very high strength stiffness and high deflectio.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® BGK-30 X PA6-(GF+GB)30 Information provided by EMS Grivory |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® HT XE 4027 nat PA*-GF30 Product description: Grivory XE 4027 natural is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamid.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAFORM C 901 MS POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBATRON L2040G3 PPS, linear, 40% glass fiber reinforced, reduced residual chlorine PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.800 - 1.60 J/cm² @Temperature -30.0 - 0.000 °C |
3.81 - 7.61 ft-lb/in² @Temperature -22.0 - 32.0 °F |
Average value: 1.23 J/cm² Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature -40.0 °C |
3.81 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Rynite® FR530L BK507 Polyethylene Terephthalate (PET) Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® G 21 PA6I/6T Product description: Grivory G 21 natural 6506 is a high viscosity, partially aromatic, amorphous copolyamide with processing aid. Improved gas and aroma barrier at elevated relative humidityExcelle.. |
|||
Charpy Impact, Notched | 0.800 J/cm² @Temperature 30.0 °C |
3.81 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-4 HY black 9205 PA6T/6I-GF40 Product description: Grivory HT1V-4 HY black 9205 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-4 HY bl.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | |
LATI Latilub 66-15ST G/30 PA66, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® GH-25 Acetal Co-polymer (POM), GF 25% reinforced, High strength, High rigidity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |