Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.221 J/cm² | 1.05 ft-lb/in² | ASTM D256 |
Plenco 00732 Melamine-Phenolic, Granular, Compression Molded PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007.. |
|||
Charpy Impact, Notched | 0.221 J/cm² | 1.05 ft-lb/in² | ASTM D256 |
Plenco 00755 Melamine-Phenolic, Granular, Compression Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |