Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.160 - 0.260 J/cm² | 0.761 - 1.24 ft-lb/in² | Average value: 0.196 J/cm² Grade Count:15 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Charpy Impact, Notched | 0.144 - 0.260 J/cm² | 0.685 - 1.24 ft-lb/in² | Average value: 0.178 J/cm² Grade Count:8 |