Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVASTER® B BT Polyethylene Terephthalate FeaturesPBT basic type for injection moulding. Melt is characterized by outstanding fluidity, which enables injection moulding of complicated and divided products also on multiple moulds. Anisotro.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Charpy Impact, Notched | >= 0.160 J/cm² | >= 0.761 ft-lb/in² | ISO 179 |
Perstorp Compounds 161 Urea-Formaldehyde w/ cellulose filler Perstorp 161 compression grade has low shrinkage, low water absorption and high strength. It is suitable for circuit breakers and electrical accessories in humid environments.Information provided by.. |
|||
Charpy Impact, Notched | >= 0.160 J/cm² | >= 0.761 ft-lb/in² | ISO 179 |
Perstorp Compounds 371 Urea-Formaldehyde w/ cellulose filler Information provided by Perstorp Compounds Inc. |
|||
Charpy Impact, Notched | 0.160 - 7.50 J/cm² | 0.761 - 35.7 ft-lb/in² | Average value: 1.35 J/cm² Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Charpy Impact, Notched | 0.160 - 4.50 J/cm² | 0.761 - 21.4 ft-lb/in² | Average value: 0.723 J/cm² Grade Count:35 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B FRN 3 LS PBT, flame retarder, light stable FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B FRN 3 PBT, flame retarder FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Charpy Impact, Notched | 0.160 - 0.260 J/cm² | 0.761 - 1.24 ft-lb/in² | Average value: 0.196 J/cm² Grade Count:15 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ 151733 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Contact strips.Information provided by Bak AGBak AG became a part of Hexion in 20.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Keripol® RZ 1141 Polyester Molding Compound, High Surface Quality Polyester molding compound, organically/inorganically filled, glass fiber reinforced, styrene free, very slight post shrinkage, processing shrinkage as for phenolic molding compounds, high surface q.. |
|||
Charpy Impact, Notched | 0.160 J/cm² | 0.761 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 200FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, Super High Flow DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.160 J/cm² | 0.761 ft-lb/in² | ISO 179/1eA |
Polyplastics TOPAS® 5013 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) This grade is characterized by its high flowability and superior optical properties. It is suitable for optical components such as lenses and light guide panels where high molded precision is indisp.. |
|||
Charpy Impact, Notched | 0.160 J/cm² | 0.761 ft-lb/in² | ISO 179/1eA |
Polyplastics TOPAS® 6015 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) A similar grade to 6013. However, heat deflection temperature is (HDT/B) = 150°C. This is a temperature that cannot be achieved with many other amorphous polymers.Information provided by PolyPlasti.. |
|||
Charpy Impact, Notched | 0.160 J/cm² | 0.761 ft-lb/in² | ISO 179/1eA |
Polyplastics TOPAS® 6017 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Possesses the highest heat resistance among cyclic olefin-type resins.Information provided by PolyPlastics. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC) TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high .. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture.. |
|||
Charpy Impact, Notched | 0.160 J/cm² | 0.761 ft-lb/in² | ISO 179 |
Unitika TERRAMAC TE-2000 Polylactic Acid (PLA) Basic grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 0.160 J/cm² | 0.761 ft-lb/in² | ISO 179 |
Unitika TERRAMAC TP-4000 Polylactic Acid (PLA) Basic grade, Extrusion, blow, and foam sheet grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT™ 2021 Polyimide, 15% Graphite (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature -30.0 °C |
0.761 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1101 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature -30.0 °C |
0.761 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1102 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.160 - 0.480 J/cm² | 0.761 - 2.28 ft-lb/in² | Average value: 0.337 J/cm² Grade Count:11 |
Overview of materials for Polyimide, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact, Notched | 0.160 J/cm² @Temperature -30.0 °C |
0.761 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1102 L Polypropylene Data was collected by ISO methods and provided by BASF. |