Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 0.460 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.460 J/cm²

@Temperature -30.0 °C
2.19 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Nilit FRIANYL A63 SG10 Nylon 6.6 for injection molding, 10% mineral filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.460 J/cm²
2.19 ft-lb/in²
ISO 179/1eA
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded  (
AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer..
Charpy Impact, Notched 0.460 J/cm²

@Temperature 23.0 °C
2.19 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BFM40-DL04N1 Nylon 6 40% Mineral Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 0.460 J/cm²

@Temperature 23.0 °C
2.19 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BFG15-DN00N1 Nylon 6 16% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 0.460 J/cm²
2.19 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 2016 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.460 J/cm²
2.19 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 751SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.460 J/cm²
2.19 ft-lb/in²
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® FR95G25V0NH NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 ZYTEL FR95G25V0NH NC010 is 25% glass fiber reinforced flame retardant polyamide halogen and red phosphorous free with high flow and excellent long t..
Charpy Impact, Notched 0.460 J/cm²

@Temperature -30.0 °C
2.19 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-020,GB30Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Reinforce..
Charpy Impact, Notched 0.460 J/cm²

@Temperature -30.0 °C
2.19 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Conditioned)
Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good ..
Charpy Impact, Notched 0.460 J/cm²

@Temperature -30.0 °C
2.19 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BUM 30 Nylon 11, 30% Glass Bead Filled (Conditioned)
Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High comp..
Copyright © lookpolymers.com All Rights Reserved