Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 0.630 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.630 J/cm²

@Temperature 22.8 °C
3.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
Charpy Impact, Notched 0.630 J/cm²

@Temperature 22.8 °C
3.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
Charpy Impact, Notched 0.630 J/cm²

@Temperature 22.8 °C
3.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced
Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
Charpy Impact, Notched 0.630 J/cm²

@Temperature 22.8 °C
3.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-G30 Modified-PPO, 30% Glass Reinforced
Modified-Polyphenylene Oxide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
Charpy Impact, Notched 0.630 J/cm²

@Temperature 23.0 °C
3.00 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
PolyOne Bergamid™ B700 Mi10 UF Polyamide 6 (Nylon 6)
Information provided by PolyOne
Charpy Impact, Notched 0.630 - 1.89 J/cm²
3.00 - 8.99 ft-lb/in²
Average value: 1.19 J/cm² Grade Count:9
Overview of materials for Polyphenylene Ether, Heat Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu..
Charpy Impact, Notched 0.630 J/cm²

@Temperature 23.0 °C
3.00 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st..
Charpy Impact, Notched 0.630 J/cm²
3.00 ft-lb/in²
ISO 179
GEHR Plastics PEEK-mod Polyetheretherketone, 10% PTFE, 10% Graphite, 10% Carbon Fiber
Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical ..
Charpy Impact, Notched 0.630 J/cm²

@Temperature -20.0 °C
3.00 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
IRPC Polimaxx Polene 2500H Polypropylene Block Copolymer
CHARACTERISTICS: EXCELLENT HIGH IMPACT, HIGH TOUGHNESS GOOD EXTRUDABILITYAPPLICATIONS: SHEET / BLOW MOLD EXTRUSION AND INJECTION MOLDING FOR CORRUGATE SHEETS, SHEETS FOR FILE, HOUSEWARES, CONTAINERS..
Charpy Impact, Notched 0.630 J/cm²
3.00 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® CRN7015 Polybutylene Terephthalate (PBT), Low gas generation, Low contact contamination, FR, UL approved regrind 50%, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.630 J/cm²
3.00 ft-lb/in²
EN ISO 179/1eA
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut..
Charpy Impact, Notched 0.630 J/cm²
3.00 ft-lb/in²
EN ISO 179/1eA
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified
Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex
Charpy Impact, Notched 0.630 - 1.40 J/cm²
3.00 - 6.66 ft-lb/in²
Average value: 0.826 J/cm² Grade Count:8
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..
Copyright © lookpolymers.com All Rights Reserved