Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.800 - 1.40 J/cm²
3.81 - 6.66 ft-lb/in²
Average value: 1.14 J/cm² Grade Count:17
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Charpy Impact, Notched 0.350 - 1.40 J/cm²
1.67 - 6.66 ft-lb/in²
Average value: 0.836 J/cm² Grade Count:5
Overview of materials for Polyphenylene Ether, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ..
Charpy Impact, Notched 0.300 - 1.40 J/cm²

@Temperature -40.0 - -30.0 °C
1.43 - 6.66 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.804 J/cm² Grade Count:49
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Charpy Impact, Notched 0.500 - 1.40 J/cm²
2.38 - 6.66 ft-lb/in²
Average value: 0.850 J/cm² Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Charpy Impact, Notched 0.500 - 1.40 J/cm²
2.38 - 6.66 ft-lb/in²
Average value: 0.800 J/cm² Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Charpy Impact, Notched 0.410 - 1.40 J/cm²
1.95 - 6.66 ft-lb/in²
Average value: 0.675 J/cm² Grade Count:4
Overview of materials for Nylon 12, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr..
Charpy Impact, Notched 1.26 - 1.40 J/cm²
6.00 - 6.66 ft-lb/in²
Average value: 1.31 J/cm² Grade Count:3
Overview of materials for Nylon 12, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Charpy Impact, Notched 0.280 - 1.40 J/cm²
1.33 - 6.66 ft-lb/in²
Average value: 0.715 J/cm² Grade Count:11
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Charpy Impact, Notched 0.600 - 1.40 J/cm²
2.86 - 6.66 ft-lb/in²
Average value: 0.830 J/cm² Grade Count:10
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Charpy Impact, Notched 0.630 - 1.40 J/cm²
3.00 - 6.66 ft-lb/in²
Average value: 0.826 J/cm² Grade Count:8
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..
Charpy Impact, Notched 1.10 - 1.40 J/cm²
5.24 - 6.66 ft-lb/in²
Average value: 1.24 J/cm² Grade Count:5
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is ..
Charpy Impact, Notched 1.10 - 1.40 J/cm²

@Temperature -30.0 - -30.0 °C
5.24 - 6.66 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.24 J/cm² Grade Count:5
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is ..
Charpy Impact, Notched 0.0400 - 1.40 J/cm²

@Temperature -30.0 - -20.0 °C
0.190 - 6.66 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.266 J/cm² Grade Count:30
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 0.200 - 1.40 J/cm²
0.952 - 6.66 ft-lb/in²
Average value: 0.514 J/cm² Grade Count:19
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Charpy Impact, Notched 0.600 - 1.40 J/cm²

@Temperature -40.0 - -30.0 °C
2.86 - 6.66 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.850 J/cm² Grade Count:7
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Charpy Impact, Notched 0.900 - 1.40 J/cm²
4.28 - 6.66 ft-lb/in²
Average value: 1.11 J/cm² Grade Count:8
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
Charpy Impact, Notched 0.900 - 1.40 J/cm²

@Temperature -30.0 - -30.0 °C
4.28 - 6.66 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.08 J/cm² Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
Charpy Impact, Notched 0.600 - 1.40 J/cm²
2.86 - 6.66 ft-lb/in²
Average value: 0.929 J/cm² Grade Count:32
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..
Charpy Impact, Notched 0.800 - 1.40 J/cm²
3.81 - 6.66 ft-lb/in²
Average value: 1.01 J/cm² Grade Count:30
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..