Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.179 J/cm² | 0.852 ft-lb/in² | ASTM D256 |
Plenco 05118-T5 Phenolic, Granular, Compression Molded PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, ve.. |
|||
Charpy Impact, Notched | 0.179 J/cm² | 0.852 ft-lb/in² | ASTM D256 |
Plenco 2000 Phenolic, Granular, Injection Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |