Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.990 J/cm²
4.71 ft-lb/in²
ISO 179
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA), 45% Glass Fiber
Amodel® A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient..
Charpy Impact, Notched 0.990 J/cm²
4.71 ft-lb/in²
ISO 179
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA), 45% Glass Fiber
Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Flow; High Stiffn..
Charpy Impact, Notched 0.990 J/cm²
4.71 ft-lb/in²
ISO 179/1eA
DuPont Performance Polymers Crastin® SK695FR NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate  Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b..
Charpy Impact, Notched 0.990 J/cm²
4.71 ft-lb/in²
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 330 NC010 Nylon  (Unverified Data**)
Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 0.990 J/cm²

@Temperature -30.0 °C
4.71 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric..
Charpy Impact, Notched 0.990 J/cm²

@Temperature -30.0 °C
4.71 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® KMVO 39099 TL Nylon 11 (Dry)
Designation ISO 1874-PA11,MHL,18-010Steel gray rigid grade for injection molding. Available color: natural. Light and heat stabilized.Low shrinkage: include 1% on average for the design of the mold...
Charpy Impact, Notched 0.990 J/cm²
4.71 ft-lb/in²
ISO 179
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of ..
Charpy Impact, Notched 0.990 J/cm²
4.71 ft-lb/in²
ISO 179
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade. - Natural: HFZ A-1145 L NT - Black: HFZ A-1145 L BK 937Information provided by Solvay Specialty Polymers.