Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.990 J/cm² | 4.71 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA), 45% Glass Fiber Amodel® A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient.. |
|||
Charpy Impact, Notched | 0.990 J/cm² | 4.71 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA), 45% Glass Fiber Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; High Flow; High Stiffn.. |
|||
Charpy Impact, Notched | 0.990 J/cm² | 4.71 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® SK695FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |
|||
Charpy Impact, Notched | 0.990 J/cm² | 4.71 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.990 J/cm² @Temperature -30.0 °C |
4.71 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric.. |
|||
Charpy Impact, Notched | 0.990 J/cm² @Temperature -30.0 °C |
4.71 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® KMVO 39099 TL Nylon 11 (Dry) Designation ISO 1874-PA11,MHL,18-010Steel gray rigid grade for injection molding. Available color: natural. Light and heat stabilized.Low shrinkage: include 1% on average for the design of the mold... |
|||
Charpy Impact, Notched | 0.990 J/cm² | 4.71 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Amodel® A-1145 DW Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 DW is a 45% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of .. |
|||
Charpy Impact, Notched | 0.990 J/cm² | 4.71 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Amodel® HFZ A-1145 L Polyphthalamide (PPA)
(Unverified Data**) Amodel® HFZ A-1145 L is a high-flow, 45% glass-fiber-reinforced grade. - Natural: HFZ A-1145 L NT - Black: HFZ A-1145 L BK 937Information provided by Solvay Specialty Polymers. |