Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.150 - 0.250 J/cm² @Temperature 23.0 °C |
0.714 - 1.19 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eA |
Raschig Group 3536 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Charpy Impact, Notched | 0.150 - 0.250 J/cm² @Temperature 23.0 °C |
0.714 - 1.19 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eA |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Charpy Impact, Notched | 0.150 - 0.250 J/cm² | 0.714 - 1.19 ft-lb/in² | ISO 179/1eA |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Charpy Impact, Notched | 0.150 - 0.250 J/cm² | 0.714 - 1.19 ft-lb/in² | ISO 179/1eA |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Charpy Impact, Notched | 0.150 - 0.250 J/cm² | 0.714 - 1.19 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Charpy Impact, Notched | 0.200 - 0.250 J/cm² | 0.952 - 1.19 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group RALUPOL® 4566 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Charpy Impact, Notched | 0.178 - 0.249 J/cm² | 0.847 - 1.19 ft-lb/in² | Average value: 0.196 J/cm² Grade Count:25 |
Overview of materials for Phenolic, Novolac, Woodflour Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact, Notched | 0.205 - 0.251 J/cm² | 0.976 - 1.19 ft-lb/in² | Average value: 0.222 J/cm² Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact, Notched | 0.150 - 0.250 J/cm² | 0.714 - 1.19 ft-lb/in² | ISO 179 |
Vyncolit 3520 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |