Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.41 J/cm² | 6.71 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, DRY Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe.. |
|||
Charpy Impact, Notched | 1.41 J/cm² | 6.71 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, Conditioned Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr.. |