Mechanical Properties Metric English Comments
Charpy Impact, Notched 2.31 J/cm²
11.0 ft-lb/in²
ASTM D256
Plenco 08112 Polyester BMC, Compression Molded
PLENCO 08112 is a renumber of PlasGlas 10112. PLENCO 08112 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co..
Charpy Impact, Notched 2.32 J/cm²
11.0 ft-lb/in²
Arkema Group Rilsan® AZM 50 NOIR T6LD Nylon 12, 50% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid..