Mechanical Properties Metric English Comments
Charpy Impact, Notched 4.20 J/cm²
20.0 ft-lb/in²
ISO 179
Iran Petrochemical (PCC) BL6 HM7255 High Density Polyethylene
BL6 (HM 755) is a high density polyethylene with Butene-1 as a comonomer. It is a high molar mass material with very good impact strength, stiffness, and stress cracking resistance.Applications: la..
Charpy Impact, Notched 4.20 J/cm²
20.0 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® ST25G7 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
Charpy Impact, Notched 4.20 J/cm²
20.0 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® TD642 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
Charpy Impact, Notched 4.20 J/cm²
20.0 ft-lb/in²
ISO 179/1eA
Borealis Daplen™ EE040AE TPO Compound
Daplen EE040AE is an elastomer modified polypropylene compound intended for injection molding. Daplen EE040AE is a material with excellent impact /stiffness ratio. Thanks to its low thermal expansi..
Charpy Impact, Notched 4.20 J/cm²

@Temperature 23.0 °C
20.0 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6000/58 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Impact Modified Until -40°C, UV Stabilized, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact, Notched 4.20 J/cm²
20.0 ft-lb/in²
DIN 53453, Ductile break
DSM Fibre Intermediates Nyrim® 1500 (Conditioned)
Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc..
Charpy Impact, Notched 4.20 J/cm²
20.0 ft-lb/in²
DIN 53453, Ductile break
DSM Fibre Intermediates Nyrim® 3000 (Dry)
Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec..