Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.400 - 5.50 J/cm²

@Temperature -30.0 - 0.000 °C
1.90 - 26.2 ft-lb/in²

@Temperature -22.0 - 32.0 °F
Average value: 2.45 J/cm² Grade Count:64
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Charpy Impact, Notched 2.00 - 5.50 J/cm²

@Temperature -30.0 - -30.0 °C
9.52 - 26.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.50 J/cm² Grade Count:5
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Charpy Impact, Notched 0.600 - 5.50 J/cm²

@Temperature -30.0 - -30.0 °C
2.86 - 26.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.58 J/cm² Grade Count:17
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Charpy Impact, Notched 0.200 - 5.50 J/cm²
0.952 - 26.2 ft-lb/in²
Average value: 0.635 J/cm² Grade Count:54
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..