Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.400 - 0.770 J/cm² @Temperature -30.0 - -20.0 °C |
1.90 - 3.66 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.647 J/cm² Grade Count:12 |