Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.840 J/cm²
4.00 ft-lb/in²
ISO 179/1eA
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin
Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim
Charpy Impact, Notched 0.840 J/cm²
4.00 ft-lb/in²
ISO 179/1eA
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin
Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati..
Charpy Impact, Notched 0.840 J/cm²

@Temperature 22.8 °C
4.00 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
Charpy Impact, Notched 0.840 J/cm²

@Temperature 23.0 °C
4.00 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
PolyOne Bergamid™ B700 G20 H UF Polyamide 6 (Nylon 6)
Information provided by PolyOne
Charpy Impact, Notched 0.840 J/cm²

@Temperature 23.0 °C
4.00 ft-lb/in²

@Temperature 73.4 °F
ISO 179
PolyOne Edgetek® NJ-30GF/000 natural Polyamide 12 (Nylon 12)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Charpy Impact, Notched 0.840 J/cm²

@Temperature -30.0 °C
4.00 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Orgalloy® RS 6020 Nylon 6 Alloy, 20% Glass Fiber (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties...
Charpy Impact, Notched 0.840 J/cm²
4.00 ft-lb/in²
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® FR50 BK505 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 BK505 is a 25% glass fiber reinforced flame retardant black polyamide 66 resin for injection molding.Information provided by DuPont Perfo..