Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179/1eA |
Radici Radiflam® ARV300 AE (dry) Nylon 66 PA66 Self-extinguishing glass-fiber reinforced with halogensInformation provided by Radici group. |
|||
Charpy Impact, Notched | 0.950 J/cm² @Temperature 23.0 °C |
4.52 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S RCV3515 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.950 J/cm² @Temperature 23.0 °C |
4.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
PolyOne Bergadur™ PB40 G20 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.950 - 1.30 J/cm² @Temperature -30.0 - -20.0 °C |
4.52 - 6.19 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 1.06 J/cm² Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179/1eA |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi.. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, Conditioned Description: Flame retardant Polyamide PA66 reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This R.. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers KetaSpire® KT-820 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber KetaSpire® KT-820 GF15 is a low flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpir.. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179/1eA |
Borealis Xmod™ GD301HP High Performance 32% Glass Fiber Reinforced Xmod GD301HP is reinforced with 32% chemically coupled glass fibers and based on specific Polymer matrix material which is bringing excellent mechanical properties (impact behavior) and very good st.. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | Bayer Test |
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 30 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Charpy Impact, Notched | 0.950 J/cm² @Temperature -30.0 °C |
4.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Charpy Impact, Notched | 0.950 J/cm² @Temperature -30.0 °C |
4.52 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AZM 23 G9 T6LD Nylon 12, 23% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-050,(G+C)(F+D)(23+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | cond.; ISO 179 1eA |
Azoty Tarnow™ Tarnamid® T-27 GF15 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 15% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBATER B512A PBT unreinforced, flame retardant PBT FR(17)Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.950 J/cm² @Temperature 23.0 °C |
4.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Charpy Impact, Notched | 0.950 J/cm² @Thickness 6.00 mm |
4.52 ft-lb/in² @Thickness 0.236 in |
ISO 179 |
Ashley Polymers Ashlene® ABS Resin 223 Medium impact, medium flow, matte finish. Suitable for general purpose injection molding.Data provided by the manufacturer |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® HN301-G20 PA6 Resin 20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179/IeA |
Addiplast Addilene J 520 T30 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179/IeA |
Addiplast Addinyl A2H V25 Flame Retardant Nylon 66, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.950 J/cm² @Temperature 23.0 °C |
4.52 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm, r=0.25; V-notch; ISO 179/1eA |
SYNTHOS Krasten® 562E High Impact Polystyrene High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of plates, sheets, technical parts and molded packaging (used in e.g. the fo.. |
|||
Charpy Impact, Notched | 0.950 J/cm² | 4.52 ft-lb/in² | ISO 179/IeA |
Addiplast Addinyl B25 V25 Flame Retardant Nylon 6, 25% Glass Filled Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.950 J/cm² @Temperature 23.0 °C |
4.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, .. |