Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.950 - 1.30 J/cm²

@Temperature -30.0 - -20.0 °C
4.52 - 6.19 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 1.06 J/cm² Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Charpy Impact, Notched 0.310 - 1.30 J/cm²

@Temperature -30.0 - 30.0 °C
1.48 - 6.19 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.05 J/cm² Grade Count:11
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Charpy Impact, Notched 0.300 - 1.30 J/cm²

@Temperature -30.0 - -20.0 °C
1.43 - 6.19 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.774 J/cm² Grade Count:27
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Charpy Impact, Notched 0.300 - 1.30 J/cm²

@Temperature -30.0 - -20.0 °C
1.43 - 6.19 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.744 J/cm² Grade Count:9
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Charpy Impact, Notched 0.500 - 1.30 J/cm²
2.38 - 6.19 ft-lb/in²
Average value: 0.877 J/cm² Grade Count:26
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Charpy Impact, Notched 0.400 - 1.30 J/cm²
1.90 - 6.19 ft-lb/in²
Average value: 0.700 J/cm² Grade Count:3
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v..
Charpy Impact, Notched 0.400 - 1.30 J/cm²

@Temperature -30.0 - -30.0 °C
1.90 - 6.19 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.635 J/cm² Grade Count:4
Overview of materials for Nylon 12, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr..
Charpy Impact, Notched 1.06 - 1.30 J/cm²

@Temperature -30.0 - 30.0 °C
5.04 - 6.19 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.14 J/cm² Grade Count:3
Overview of materials for Nylon 12, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Charpy Impact, Notched 0.900 - 1.30 J/cm²

@Temperature -30.0 - -30.0 °C
4.28 - 6.19 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.14 J/cm² Grade Count:8
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Charpy Impact, Notched 0.900 - 1.30 J/cm²
4.28 - 6.19 ft-lb/in²
Average value: 1.01 J/cm² Grade Count:6
Overview of materials for Nylon 6, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria..
Charpy Impact, Notched 0.500 - 1.30 J/cm²
2.38 - 6.19 ft-lb/in²
Average value: 0.810 J/cm² Grade Count:4
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..