Polymer Property : Charpy Impact, Notched = 5.95 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.25 J/cm²

@Temperature 23.0 °C
5.95 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BFG30-FH00B2 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 1.25 J/cm²
5.95 ft-lb/in²
ISO 179/1eA
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized..
Charpy Impact, Notched 1.25 J/cm²
5.95 ft-lb/in²
Arkema Group Orgalloy® LE 60THM Flexible Nylon Alloy (Conditioned)
LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).higher in rigidity than LE 6000. For film, hollow vessel blow moldi..
Charpy Impact, Notched 1.25 J/cm²
5.95 ft-lb/in²
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric..
Charpy Impact, Notched 1.25 J/cm²

@Temperature -30.0 °C
5.95 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® MB 3750 Nylon 11, Transparent Grade (Conditioned)
Designation ISO 1874-PA11/xx,F,THL,22-020Transparent semi-crystalline PA11 grade.Used for film extrusion and injection molding (low thickness).Very good low temperature impact strength.High chemical..
Charpy Impact, Notched 1.25 J/cm² - NB
5.95 ft-lb/in² - NB
Average value: 4.72 J/cm² Grade Count:3
Overview of materials for Nylon, Flexible Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri..