Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.500 - 1.33 J/cm² @Temperature -30.0 - 30.0 °C |
2.38 - 6.33 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 0.676 J/cm² Grade Count:6 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |