Charpy Impact, Notched 1.45 J/cm²
6.90 ft-lb/in²
Arkema Group Rilsan® ASR 30 Nylon 12, 30% Carbon Fiber Filled (Dry)
Designation ISO 1874-PA12,M,16-120,CF30Rigid grade with carbon fiber filler (30%) for injection molding. Available color: black.Very high rigidity. High strength-to-weight ratio. Very low shrinkage:..
Charpy Impact, Notched 1.45 J/cm²
6.90 ft-lb/in²
Eastman Tenite 525-10 CAB Cellulose Acetate Butyrate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.