Polymer Property : Charpy Impact, Notched = 7.33 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.54 J/cm²
7.33 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® TD-25 Acetal Co-polymer (POM), High impact, Flexible
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Charpy Impact, Notched 1.54 J/cm²
7.33 ft-lb/in²
Arkema Group Pebax® 7233 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 72 shore D Highest modulus PEBAX Applications: medical, extrusion SportISO data provided by the manufacturer, Arkema.