Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS PC+ABS Recycle Resin with good flow, good temperature resistance and moderate impact |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Radici Radilon® SLVHPL128 (dry) Nylon 6 Plasticized for improved flexibilityInformation provided by Radici group. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 L-HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa SINKRAL B620 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-25-20 High impact injection moulding grade. Its` excellent balance of mechanical properties (toughness -.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | |
Ineos ABS Lustran® M201AS Increased chemical resistance compared to P2x, contains antistatic additives.,Property data per ISO test methods. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, Conditioned Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 V43 Black 21 N PA66, 43% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 43% of glass fiber, heat stabilized, for injection molding.Available in: North AmericaProduct Applications: TECHNYL® A 218 V43 is used in all sectors .. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179 |
Solvay TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 0 Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stabilityColors: it is supplied in natural color and black color.Available in: Latin America.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | 80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC STAMAX 30YM240 PP SABIC® STAMAX 30YM240 is a 30% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16496906... |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179 |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO Data |
Styron Magnum™ 9010 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Europe-Africa-Middle East) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PX1134 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1134 is an unfilled material with a Vicat B/120 of 120°C according ISO 306. NORYL PX1134 offers improved impact performance to meet the standard ECE dashboard impact tests in the automoti.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, Conditioned Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179-1 |
Unitika A1022GFL60 PA6, 60% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179-1 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Ductile Failure; ASTM D256B |
Elastomer Engineering Elastamide 200 Elastomer Modified RIM Nylon 6 26% crystallinity. Information supplied by Elastomer Engineering. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW200F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW241F12 (DAM) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® LV-50H FWA black 9225 PA12-GF50 Product description: Grilamid LV-50H FWA black 9225 is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50 Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 30.0 °C |
9.04 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-40 PA6-GF40 Product description: Grilon BGZ-40 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 40% glass fibers. Grilon BGZ-40 has the following important properties:.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARFLEN SG-1 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |